Allgemein
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Biegefestigkeit | 23.0 °C | 130 MPa Show Supplier Material materials with Biegefestigkeit of 130 MPa | ASTM D790 |
Biegemodul | 23.0 °C | 3.8 GPa Show Supplier Material materials with Biegemodul of 3.8 GPa | ASTM D790 |
Dehnung | 23.0 °C | 10 % Show Supplier Material materials with Dehnung of 10 % | max., ASTM D638 |
Hardness, Rockwell R | 23.0 °C | 110 [-] Show Supplier Material materials with Hardness, Rockwell R of 110 [-] | ASTM D785 |
Impact strength, Izod notched, ASTM | 23.0 °C | 100 J/m Show Supplier Material materials with Impact strength, Izod notched, ASTM of 100 J/m | ASTM D256 |
Zugfestigkeit | 23.0 °C | 75 MPa Show Supplier Material materials with Zugfestigkeit of 75 MPa | ASTM D638 |
Thermisch
Rheological Properties
Property | Temperature | Value | Comment |
---|---|---|---|
Schrumpfung | 23.0 °C | 0.2 - 0.8 % Show Supplier Material materials with Schrumpfung of 0.2 - 0.8 % | ASTM D955 |
Technological properties
Property | ||
---|---|---|
Application areas | Electrical and Pneumatic Hand Tools- Anti-Static handle | |
Color | Natural |