Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 1.38 g/cm³ Show Supplier Material materials with Dichte of 1.38 g/cm³ | ASTM D792 |
Wasseraufnahme, Gleichgewicht | 23.0 °C | 0.3 % Show Supplier Material materials with Wasseraufnahme, Gleichgewicht of 0.3 % | max., ASTM D4442 |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Biegefestigkeit | 23.0 °C | 220 MPa Show Supplier Material materials with Biegefestigkeit of 220 MPa | ASTM D790 |
Biegemodul | 23.0 °C | 3 GPa Show Supplier Material materials with Biegemodul of 3 GPa | ASTM D790 |
Dehnung | 23.0 °C | 5 % Show Supplier Material materials with Dehnung of 5 % | max., ASTM D638 |
Hardness, Rockwell R | 23.0 °C | 115 [-] Show Supplier Material materials with Hardness, Rockwell R of 115 [-] | ASTM D785 |
Impact strength, Izod notched, ASTM | 23.0 °C | 150 J/m Show Supplier Material materials with Impact strength, Izod notched, ASTM of 150 J/m | ASTM D256 |
Zugfestigkeit | 23.0 °C | 135 MPa Show Supplier Material materials with Zugfestigkeit of 135 MPa | ASTM D638 |
Thermisch
Rheological Properties
Property | Temperature | Value | Comment |
---|---|---|---|
Schrumpfung | 23.0 °C | 0.3 - 0.8 % Show Supplier Material materials with Schrumpfung of 0.3 - 0.8 % | ASTM D955 |
Technological properties
Property | ||
---|---|---|
Application areas | Industrial parts & Components-Water Pump | |
Color | Black | |
Fillers | 35% Glass Fiber |