Allgemein
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Biegefestigkeit | 23.0 °C | 85 MPa Show Supplier Material materials with Biegefestigkeit of 85 MPa | ASTM D790 |
Biegemodul | 23.0 °C | 2 GPa Show Supplier Material materials with Biegemodul of 2 GPa | ASTM D790 |
Dehnung | 23.0 °C | 20 % Show Supplier Material materials with Dehnung of 20 % | min., ASTM D638 |
Härte, Shore D | 23.0 °C | 72 [-] Show Supplier Material materials with Härte, Shore D of 72 [-] | ASTM D2240 |
Impact strength, Izod notched, ASTM | -30.0 °C | 50 J/m Show Supplier Material materials with Impact strength, Izod notched, ASTM of 50 J/m | min., ASTM D256 |
23.0 °C | 100 J/m Show Supplier Material materials with Impact strength, Izod notched, ASTM of 100 J/m | min., ASTM D256 | |
Zugfestigkeit | 23.0 °C | 50 MPa Show Supplier Material materials with Zugfestigkeit of 50 MPa | ASTM D638 |
Thermisch
Property | Value | Comment |
---|---|---|
Heat deflection temperature, 1.80 MPa | 50 °C Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 50 °C | ASTM D648 |
Rheological Properties
Property | Temperature | Value | Comment |
---|---|---|---|
Schmelzmassenflussrate | 50 g/10min Show Supplier Material materials with Schmelzmassenflussrate of 50 g/10min | min., ASTM D1238 | |
Schrumpfung | 23.0 °C | 1.6 - 2 % Show Supplier Material materials with Schrumpfung of 1.6 - 2 % | ASTM D955 |
Technological properties
Property | ||
---|---|---|
Application areas | Sporting Goods-Water Bottle Cages | |
Color | Black |