Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 1.21 g/cm³ Show Supplier Material materials with Dichte of 1.21 g/cm³ | ASTM D792 |
Wasseraufnahme, Gleichgewicht | 23.0 °C | 0.3 % Show Supplier Material materials with Wasseraufnahme, Gleichgewicht of 0.3 % | max., ASTM D4442 |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Biegefestigkeit | 23.0 °C | 120 MPa Show Supplier Material materials with Biegefestigkeit of 120 MPa | ASTM D790 |
Biegemodul | 23.0 °C | 3.47 GPa Show Supplier Material materials with Biegemodul of 3.47 GPa | ASTM D790 |
Dehnung | 23.0 °C | 5 % Show Supplier Material materials with Dehnung of 5 % | max., ASTM D638 |
Hardness, Rockwell R | 23.0 °C | 100 [-] Show Supplier Material materials with Hardness, Rockwell R of 100 [-] | ASTM D785 |
Impact strength, Izod notched, ASTM | 23.0 °C | 180 J/m Show Supplier Material materials with Impact strength, Izod notched, ASTM of 180 J/m | ASTM D256 |
Zugfestigkeit | 23.0 °C | 80 MPa Show Supplier Material materials with Zugfestigkeit of 80 MPa | ASTM D638 |
Thermisch
Rheological Properties
Property | Temperature | Value | Comment |
---|---|---|---|
Schrumpfung | 23.0 °C | 0.3 - 1 % Show Supplier Material materials with Schrumpfung of 0.3 - 1 % | ASTM D955 |
Technological properties
Property | ||
---|---|---|
Application areas | Electromechanical parts and accessories, Hardware, Mechanical parts, Snowshoe, Skates, Leisure sports equipment, Suitcase handle pulls | |
Color | White | |
Fillers | 15% Glass Fiber |