Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 1.17 g/cm³ Show Supplier Material materials with Dichte of 1.17 g/cm³ | ASTM D792 |
Wasseraufnahme, Gleichgewicht | 23.0 °C | 0.3 % Show Supplier Material materials with Wasseraufnahme, Gleichgewicht of 0.3 % | max., ASTM D4442 |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Biegefestigkeit | 23.0 °C | 130 MPa Show Supplier Material materials with Biegefestigkeit of 130 MPa | ASTM D790 |
Biegemodul | 23.0 °C | 3.2 GPa Show Supplier Material materials with Biegemodul of 3.2 GPa | ASTM D790 |
Dehnung | 23.0 °C | 5 % Show Supplier Material materials with Dehnung of 5 % | max., ASTM D638 |
Härte, Shore D | 23.0 °C | 77 [-] Show Supplier Material materials with Härte, Shore D of 77 [-] | ASTM D2240 |
Impact strength, Izod notched, ASTM | 23.0 °C | 30 J/m Show Supplier Material materials with Impact strength, Izod notched, ASTM of 30 J/m | ASTM D256 |
Zugfestigkeit | 23.0 °C | 70 MPa Show Supplier Material materials with Zugfestigkeit of 70 MPa | ASTM D638 |
Thermisch
Property | Value |
---|---|
Entflammbarkeit | UL 94 (1.6mm) V0 |
Rheological Properties
Property | Temperature | Value | Comment |
---|---|---|---|
Schrumpfung | 23.0 °C | 0.7 - 0.9 % Show Supplier Material materials with Schrumpfung of 0.7 - 0.9 % | ASTM D955 |
Technological properties
Property | ||
---|---|---|
Application areas | Connector, Electrical switch housing, Cooling Fan, Power tools, Machine tool motor housing, Industrial Parts & Components-Thread Spool | |
Color | Natural |