Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 1.14 g/cm³ Show Supplier Material materials with Dichte of 1.14 g/cm³ | ASTM D792 |
Wasseraufnahme, Gleichgewicht | 23.0 °C | 0.3 % Show Supplier Material materials with Wasseraufnahme, Gleichgewicht of 0.3 % | max., ASTM D4442 |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Biegefestigkeit | 23.0 °C | 120 MPa Show Supplier Material materials with Biegefestigkeit of 120 MPa | ASTM D790 |
Biegemodul | 23.0 °C | 2.8 GPa Show Supplier Material materials with Biegemodul of 2.8 GPa | ASTM D790 |
Dehnung | 23.0 °C | 2 % Show Supplier Material materials with Dehnung of 2 % | min., ASTM D638 |
Härte, Shore D | 23.0 °C | 80 [-] Show Supplier Material materials with Härte, Shore D of 80 [-] | ASTM D2240 |
Impact strength, Izod notched, ASTM | 23.0 °C | 50 J/m Show Supplier Material materials with Impact strength, Izod notched, ASTM of 50 J/m | ASTM D256 |
Zugfestigkeit | 23.0 °C | 68 MPa Show Supplier Material materials with Zugfestigkeit of 68 MPa | ASTM D638 |
Thermisch
Rheological Properties
Property | Temperature | Value | Comment |
---|---|---|---|
Schmelzmassenflussrate | 70 - 250 g/10min Show Supplier Material materials with Schmelzmassenflussrate of 70 - 250 g/10min | ASTM D1238 | |
Schrumpfung | 23.0 °C | 1.2 - 1.6 % Show Supplier Material materials with Schrumpfung of 1.2 - 1.6 % | ASTM D955 |
Technological properties
Property | ||
---|---|---|
Application areas | Washer, Baby Strollers, Electrical and electronic parts, Information technology equipment parts, Tool housing , Sports equipment, Gear, Sporting goods-Glasses temples Automobiles parts | |
Color | Black |