Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 1.07 g/cm³ Show Supplier Material materials with Dichte of 1.07 g/cm³ | ASTM D792 |
Wasseraufnahme, Gleichgewicht | 23.0 °C | 0.3 % Show Supplier Material materials with Wasseraufnahme, Gleichgewicht of 0.3 % | max., ASTM D4442 |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Biegefestigkeit | 23.0 °C | 70 MPa Show Supplier Material materials with Biegefestigkeit of 70 MPa | ASTM D790 |
Biegemodul | 23.0 °C | 1.76 GPa Show Supplier Material materials with Biegemodul of 1.76 GPa | ASTM D790 |
Dehnung | 23.0 °C | 70 % Show Supplier Material materials with Dehnung of 70 % | min., ASTM D638 |
Härte, Shore D | 23.0 °C | 80 [-] Show Supplier Material materials with Härte, Shore D of 80 [-] | ASTM D2240 |
Impact strength, Izod notched, ASTM | -30.0 °C | 200 J/m Show Supplier Material materials with Impact strength, Izod notched, ASTM of 200 J/m | min., ASTM D256 |
23.0 °C | 850 J/m Show Supplier Material materials with Impact strength, Izod notched, ASTM of 850 J/m | min., ASTM D256 | |
Zugfestigkeit | 23.0 °C | 45 MPa Show Supplier Material materials with Zugfestigkeit of 45 MPa | ASTM D638 |
Thermisch
Property | Value | Comment |
---|---|---|
Heat deflection temperature, 1.80 MPa | 50 °C Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 50 °C | ASTM D648 |
Rheological Properties
Technological properties
Property | ||
---|---|---|
Application areas | Sporting Goods-Shoe Buckle, Bicycles-Shoe buckle, Snowshoe sole, Sled, Skates. Badminton racket line pipe nails, Medical Equipment-Hospital bed caster, Sporting Goods-Glasses temples, Baby Strollers-Baby Stroller cable ties | |
Color | Natural |