Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 1.09 g/cm³ Show Supplier Material materials with Dichte of 1.09 g/cm³ | ASTM D792 |
Wasseraufnahme, Gleichgewicht | 23.0 °C | 0.3 % Show Supplier Material materials with Wasseraufnahme, Gleichgewicht of 0.3 % | max., ASTM D4442 |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Biegefestigkeit | 23.0 °C | 95 MPa Show Supplier Material materials with Biegefestigkeit of 95 MPa | ASTM D790 |
Biegemodul | 23.0 °C | 2.3 GPa Show Supplier Material materials with Biegemodul of 2.3 GPa | ASTM D790 |
Dehnung | 23.0 °C | 50 % Show Supplier Material materials with Dehnung of 50 % | min., ASTM D638 |
Härte, Shore D | 23.0 °C | 78 [-] Show Supplier Material materials with Härte, Shore D of 78 [-] | ASTM D2240 |
Impact strength, Izod notched, ASTM | 23.0 °C | 100 J/m Show Supplier Material materials with Impact strength, Izod notched, ASTM of 100 J/m | ASTM D256 |
Zugfestigkeit | 23.0 °C | 55 MPa Show Supplier Material materials with Zugfestigkeit of 55 MPa | ASTM D638 |
Rheological Properties
Property | Temperature | Value | Comment |
---|---|---|---|
Schrumpfung | 23.0 °C | 0.8 - 1.1 % Show Supplier Material materials with Schrumpfung of 0.8 - 1.1 % | ASTM D955 |
Technological properties
Property | ||
---|---|---|
Application areas | Sports equipment, Buckle | |
Color | Natural |