Allgemein
Property | Temperature | Value |
---|---|---|
Dichte | 23.0 °C | 8.4 g/cm³ Show Supplier Material materials with Dichte of 8.4 g/cm³ |
Abmessung
Property | Value |
---|---|
Dimensions | Sheet Thickness: 0.3 - 8 mm, Foil Thickness: 0.005-0.45 mm |
Mechanisch
Property | Temperature | Value |
---|---|---|
Dehnung A5 | 23.0 °C | 12 % Show Supplier Material materials with Dehnung A5 of 12 % |
Elastizitätsmodul | 23.0 °C | 110 GPa Show Supplier Material materials with Elastizitätsmodul of 110 GPa |
Härte, Brinell | 23.0 °C | 190 [-] Show Supplier Material materials with Härte, Brinell of 190 [-] |
Streckgrenze Rp 0,2 | 23.0 °C | 580 MPa Show Supplier Material materials with Streckgrenze Rp 0,2 of 580 MPa |
Zugfestigkeit | 23.0 °C | 610 MPa Show Supplier Material materials with Zugfestigkeit of 610 MPa |
Thermisch
Property | Temperature | Value |
---|---|---|
Koeffizient der thermischen Ausdehnung | 23.0 °C | 2.02E-5 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 2.02E-5 1/K |
Wärmeleitfähigkeit | 23.0 °C | 121 W/(m·K) Show Supplier Material materials with Wärmeleitfähigkeit of 121 W/(m·K) |
Elektrisch
Property | Temperature | Value |
---|---|---|
Elektrische Leitfähigkeit | 23.0 °C | 1.55E+7 S/m Show Supplier Material materials with Elektrische Leitfähigkeit of 1.55E+7 S/m |
Chemical properties
Property | Value |
---|---|
Aluminium | 0.05 % Show Supplier Material materials with Aluminium of 0.05 % |
Blei | 0.1 % Show Supplier Material materials with Blei of 0.1 % |
Eisen | 0.1 % Show Supplier Material materials with Eisen of 0.1 % |
Kupfer | 62 - 64 % Show Supplier Material materials with Kupfer of 62 - 64 % |
Nickel | 0.3 % Show Supplier Material materials with Nickel of 0.3 % |
Zinn | 0.1 % Show Supplier Material materials with Zinn of 0.1 % |