Allgemein
Property | Temperature | Value |
---|---|---|
Dichte | 23.0 °C | 2.7 g/cm³ Show Supplier Material materials with Dichte of 2.7 g/cm³ |
Mechanisch
Property | Temperature | Value |
---|---|---|
Dehnung A5 | 23.0 °C | 8 % Show Supplier Material materials with Dehnung A5 of 8 % |
Elastizitätsmodul | 23.0 °C | 69 GPa Show Supplier Material materials with Elastizitätsmodul of 69 GPa |
Härte, Brinell | 23.0 °C | 90 [-] Show Supplier Material materials with Härte, Brinell of 90 [-] |
Streckgrenze Rp 0,2 | 23.0 °C | 240 MPa Show Supplier Material materials with Streckgrenze Rp 0,2 of 240 MPa |
Zugfestigkeit | 23.0 °C | 290 MPa Show Supplier Material materials with Zugfestigkeit of 290 MPa |
Thermisch
Property | Temperature | Value |
---|---|---|
Koeffizient der thermischen Ausdehnung | 23.0 °C | 2.36E-5 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 2.36E-5 1/K |
Wärmeleitfähigkeit | 23.0 °C | 160 W/(m·K) Show Supplier Material materials with Wärmeleitfähigkeit of 160 W/(m·K) |
Elektrisch
Property | Temperature | Value |
---|---|---|
Elektrische Leitfähigkeit | 23.0 °C | 2.50E+7 S/m Show Supplier Material materials with Elektrische Leitfähigkeit of 2.50E+7 S/m |
Chemical properties
Property | Value |
---|---|
Aluminium | 95.9 - 98.6 % Show Supplier Material materials with Aluminium of 95.9 - 98.6 % |
Andere | 0 - 0.15 % Show Supplier Material materials with Andere of 0 - 0.15 % |
Chrom | 0.04 - 0.35 % Show Supplier Material materials with Chrom of 0.04 - 0.35 % |
Eisen | 0 - 0.7 % Show Supplier Material materials with Eisen of 0 - 0.7 % |
Kupfer | 0.15 - 0.4 % Show Supplier Material materials with Kupfer of 0.15 - 0.4 % |
Magnesium | 0.8 - 1.2 % Show Supplier Material materials with Magnesium of 0.8 - 1.2 % |
Mangan | 0 % Show Supplier Material materials with Mangan of 0 % |
Silizium | 0.4 - 0.8 % Show Supplier Material materials with Silizium of 0.4 - 0.8 % |
Titan | 0 - 0.15 % Show Supplier Material materials with Titan of 0 - 0.15 % |
Zink | 0 - 0.25 % Show Supplier Material materials with Zink of 0 - 0.25 % |