Allgemein
Property | Temperature | Value |
---|---|---|
Dichte | 23.0 °C | 2.8 g/cm³ Show Supplier Material materials with Dichte of 2.8 g/cm³ |
Mechanisch
Property | Temperature | Value |
---|---|---|
Dehnung A5 | 23.0 °C | 12 % Show Supplier Material materials with Dehnung A5 of 12 % |
Elastizitätsmodul | 23.0 °C | 72 GPa Show Supplier Material materials with Elastizitätsmodul of 72 GPa |
Härte, Brinell | 23.0 °C | 95 [-] Show Supplier Material materials with Härte, Brinell of 95 [-] |
Streckgrenze Rp 0,2 | 23.0 °C | 245 MPa Show Supplier Material materials with Streckgrenze Rp 0,2 of 245 MPa |
Zugfestigkeit | 23.0 °C | 385 MPa Show Supplier Material materials with Zugfestigkeit of 385 MPa |
Thermisch
Property | Temperature | Value |
---|---|---|
Koeffizient der thermischen Ausdehnung | 23.0 °C | 2.36E-5 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 2.36E-5 1/K |
Wärmeleitfähigkeit | 23.0 °C | 130 W/(m·K) Show Supplier Material materials with Wärmeleitfähigkeit of 130 W/(m·K) |
Elektrisch
Property | Temperature | Value |
---|---|---|
Elektrische Leitfähigkeit | 23.0 °C | 2.00E+7 S/m Show Supplier Material materials with Elektrische Leitfähigkeit of 2.00E+7 S/m |
Chemical properties
Property | Value | Comment | |
---|---|---|---|
Aluminium | Balance | ||
Andere | 0.15 % Show Supplier Material materials with Andere of 0.15 % | total, each 0.05 | |
Chrom | 0.1 % Show Supplier Material materials with Chrom of 0.1 % | ||
Eisen | 0.7 % Show Supplier Material materials with Eisen of 0.7 % | ||
Kupfer | 3.5 - 4.5 % Show Supplier Material materials with Kupfer of 3.5 - 4.5 % | ||
Magnesium | 0.4 - 1 % Show Supplier Material materials with Magnesium of 0.4 - 1 % | ||
Mangan | 0.4 - 1 % Show Supplier Material materials with Mangan of 0.4 - 1 % | ||
Silizium | 0.2 - 0.8 % Show Supplier Material materials with Silizium of 0.2 - 0.8 % | ||
Titan | 0.25 % Show Supplier Material materials with Titan of 0.25 % | max., Ti+Zr | |
Zink | 0.25 % Show Supplier Material materials with Zink of 0.25 % | ||
Zirkonium | 0.25 % Show Supplier Material materials with Zirkonium of 0.25 % | max., Ti+Zr |