Allgemein
Property | Temperature | Value |
---|---|---|
Dichte | 23.0 °C | 2.8 g/cm³ Show Supplier Material materials with Dichte of 2.8 g/cm³ |
Mechanisch
Property | Temperature | Value |
---|---|---|
Dehnung A5 | 23.0 °C | 3 % Show Supplier Material materials with Dehnung A5 of 3 % |
Elastizitätsmodul | 23.0 °C | 72 GPa Show Supplier Material materials with Elastizitätsmodul of 72 GPa |
Härte, Brinell | 23.0 °C | 140 [-] Show Supplier Material materials with Härte, Brinell of 140 [-] |
Streckgrenze Rp 0,2 | 23.0 °C | 450 MPa Show Supplier Material materials with Streckgrenze Rp 0,2 of 450 MPa |
Zugfestigkeit | 23.0 °C | 530 MPa Show Supplier Material materials with Zugfestigkeit of 530 MPa |
Thermisch
Property | Temperature | Value |
---|---|---|
Koeffizient der thermischen Ausdehnung | 23.0 °C | 2.36E-5 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 2.36E-5 1/K |
Wärmeleitfähigkeit | 23.0 °C | 130 W/(m·K) Show Supplier Material materials with Wärmeleitfähigkeit of 130 W/(m·K) |
Elektrisch
Property | Temperature | Value |
---|---|---|
Elektrische Leitfähigkeit | 23.0 °C | 1.90E+7 S/m Show Supplier Material materials with Elektrische Leitfähigkeit of 1.90E+7 S/m |
Chemical properties
Property | Value |
---|---|
Aluminium | 86.9 - 91.4 % Show Supplier Material materials with Aluminium of 86.9 - 91.4 % |
Andere | 0.15 % Show Supplier Material materials with Andere of 0.15 % |
Chrom | 0.18 - 0.28 % Show Supplier Material materials with Chrom of 0.18 - 0.28 % |
Eisen | 0.5 % Show Supplier Material materials with Eisen of 0.5 % |
Kupfer | 1.2 - 2 % Show Supplier Material materials with Kupfer of 1.2 - 2 % |
Magnesium | 2.1 - 2.9 % Show Supplier Material materials with Magnesium of 2.1 - 2.9 % |
Mangan | 0.3 % Show Supplier Material materials with Mangan of 0.3 % |
Silizium | 0.4 % Show Supplier Material materials with Silizium of 0.4 % |
Titan | 0.2 % Show Supplier Material materials with Titan of 0.2 % |
Zink | 5.1 - 6.1 % Show Supplier Material materials with Zink of 5.1 - 6.1 % |
Zirkonium | 0.25 % Show Supplier Material materials with Zirkonium of 0.25 % |