Allgemein
Property | Temperature | Value |
---|---|---|
Dichte | 23.0 °C | 2.7 g/cm³ Show Supplier Material materials with Dichte of 2.7 g/cm³ |
Mechanisch
Property | Temperature | Value |
---|---|---|
Dehnung A5 | 23.0 °C | 12 % Show Supplier Material materials with Dehnung A5 of 12 % |
Elastizitätsmodul | 23.0 °C | 69 GPa Show Supplier Material materials with Elastizitätsmodul of 69 GPa |
Härte, Brinell | 23.0 °C | 70 [-] Show Supplier Material materials with Härte, Brinell of 70 [-] |
Streckgrenze Rp 0,2 | 23.0 °C | 160 MPa Show Supplier Material materials with Streckgrenze Rp 0,2 of 160 MPa |
Zugfestigkeit | 23.0 °C | 215 MPa Show Supplier Material materials with Zugfestigkeit of 215 MPa |
Thermisch
Property | Temperature | Value |
---|---|---|
Koeffizient der thermischen Ausdehnung | 23.0 °C | 2.34E-5 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 2.34E-5 1/K |
Wärmeleitfähigkeit | 23.0 °C | 200 W/(m·K) Show Supplier Material materials with Wärmeleitfähigkeit of 200 W/(m·K) |
Elektrisch
Property | Temperature | Value |
---|---|---|
Elektrische Leitfähigkeit | 23.0 °C | 3.00E+7 S/m Show Supplier Material materials with Elektrische Leitfähigkeit of 3.00E+7 S/m |
Chemical properties
Property | Value | Comment | |
---|---|---|---|
Aluminium | Balance | ||
Andere | 0.15 % Show Supplier Material materials with Andere of 0.15 % | total, each 0.05 | |
Chrom | 0.05 % Show Supplier Material materials with Chrom of 0.05 % | ||
Eisen | 0.1 - 0.3 % Show Supplier Material materials with Eisen of 0.1 - 0.3 % | ||
Kupfer | 0.1 % Show Supplier Material materials with Kupfer of 0.1 % | ||
Magnesium | 0.35 - 0.6 % Show Supplier Material materials with Magnesium of 0.35 - 0.6 % | ||
Mangan | 0.1 % Show Supplier Material materials with Mangan of 0.1 % | ||
Silizium | 0.3 - 0.6 % Show Supplier Material materials with Silizium of 0.3 - 0.6 % | ||
Titan | 0.1 % Show Supplier Material materials with Titan of 0.1 % | ||
Zink | 0.15 % Show Supplier Material materials with Zink of 0.15 % |