Allgemein
Property | Temperature | Value |
---|---|---|
Dichte | 23.0 °C | 2.9 g/cm³ Show Supplier Material materials with Dichte of 2.9 g/cm³ |
Mechanisch
Property | Temperature | Value |
---|---|---|
Dehnung A5 | 23.0 °C | 7 % Show Supplier Material materials with Dehnung A5 of 7 % |
Elastizitätsmodul | 23.0 °C | 72 GPa Show Supplier Material materials with Elastizitätsmodul of 72 GPa |
Härte, Brinell | 23.0 °C | 100 [-] Show Supplier Material materials with Härte, Brinell of 100 [-] |
Streckgrenze Rp 0,2 | 23.0 °C | 250 MPa Show Supplier Material materials with Streckgrenze Rp 0,2 of 250 MPa |
Zugfestigkeit | 23.0 °C | 370 MPa Show Supplier Material materials with Zugfestigkeit of 370 MPa |
Thermisch
Property | Temperature | Value |
---|---|---|
Koeffizient der thermischen Ausdehnung | 23.0 °C | 2.3E-5 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 2.3E-5 1/K |
Wärmeleitfähigkeit | 23.0 °C | 130 W/(m·K) Show Supplier Material materials with Wärmeleitfähigkeit of 130 W/(m·K) |
Elektrisch
Property | Temperature | Value |
---|---|---|
Elektrische Leitfähigkeit | 23.0 °C | 2.00E+7 S/m Show Supplier Material materials with Elektrische Leitfähigkeit of 2.00E+7 S/m |
Chemical properties
Property | Value |
---|---|
Aluminium | Balance |
Bismut | 0.2 % Show Supplier Material materials with Bismut of 0.2 % |
Blei | 0.8 - 1.5 % Show Supplier Material materials with Blei of 0.8 - 1.5 % |
Chrom | 0.1 % Show Supplier Material materials with Chrom of 0.1 % |
Eisen | 0.8 % Show Supplier Material materials with Eisen of 0.8 % |
Kupfer | 3.3 - 4.6 % Show Supplier Material materials with Kupfer of 3.3 - 4.6 % |
Magnesium | 0.4 - 1.8 % Show Supplier Material materials with Magnesium of 0.4 - 1.8 % |
Mangan | 0.5 - 1 % Show Supplier Material materials with Mangan of 0.5 - 1 % |
Nickel | 0.2 % Show Supplier Material materials with Nickel of 0.2 % |
Silizium | 0.8 % Show Supplier Material materials with Silizium of 0.8 % |
Titan | 0.2 % Show Supplier Material materials with Titan of 0.2 % |
Zink | 0.8 % Show Supplier Material materials with Zink of 0.8 % |
Zinn | 0.2 % Show Supplier Material materials with Zinn of 0.2 % |