Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 7.8 g/cm³ Show Supplier Material materials with Dichte of 7.8 g/cm³ | typical for steels |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Dehnung A5 | 23.0 °C | 30 - 40 % Show Supplier Material materials with Dehnung A5 of 30 - 40 % | |
Elastizitätsmodul | 23.0 °C | 200 - 210 GPa Show Supplier Material materials with Elastizitätsmodul of 200 - 210 GPa | typical for steels |
Härte, Brinell | 23.0 °C | 215 [-] Show Supplier Material materials with Härte, Brinell of 215 [-] | |
Streckgrenze Rp 0,2 | 23.0 °C | 200 MPa Show Supplier Material materials with Streckgrenze Rp 0,2 of 200 MPa | |
Zugfestigkeit | 23.0 °C | 500 - 700 MPa Show Supplier Material materials with Zugfestigkeit of 500 - 700 MPa |
Chemical properties
Property | Value |
---|---|
Chrom | 16 - 19 % Show Supplier Material materials with Chrom of 16 - 19 % |
Eisen | 59.8 - 72 % Show Supplier Material materials with Eisen of 59.8 - 72 % |
Kohlenstoff | 0.03 % Show Supplier Material materials with Kohlenstoff of 0.03 % |
Mangan | 2 % Show Supplier Material materials with Mangan of 2 % |
Molybdän | 2 - 3 % Show Supplier Material materials with Molybdän of 2 - 3 % |
Nickel | 10 - 15 % Show Supplier Material materials with Nickel of 10 - 15 % |
Phosphor | 0.05 % Show Supplier Material materials with Phosphor of 0.05 % |
Schwefel | 0.03 % Show Supplier Material materials with Schwefel of 0.03 % |
Silizium | 1 % Show Supplier Material materials with Silizium of 1 % |
Stickstoff | 0.1 % Show Supplier Material materials with Stickstoff of 0.1 % |