Chemical properties
Property | Value |
---|---|
Bor | 1.5E-3 - 5E-3 % Show Supplier Material materials with Bor of 1.5E-3 - 5E-3 % |
Chrom | 16 - 18.5 % Show Supplier Material materials with Chrom of 16 - 18.5 % |
Eisen | 61.2 - 71.9 % Show Supplier Material materials with Eisen of 61.2 - 71.9 % |
Kohlenstoff | 0.04 % Show Supplier Material materials with Kohlenstoff of 0.04 % |
Mangan | 2 % Show Supplier Material materials with Mangan of 2 % |
Molybdän | 2 - 3 % Show Supplier Material materials with Molybdän of 2 - 3 % |
Nickel | 10 - 14 % Show Supplier Material materials with Nickel of 10 - 14 % |
Phosphor | 0.05 % Show Supplier Material materials with Phosphor of 0.05 % |
Schwefel | 0.03 % Show Supplier Material materials with Schwefel of 0.03 % |
Silizium | 1 % Show Supplier Material materials with Silizium of 1 % |
Stickstoff | 0.1 - 0.22 % Show Supplier Material materials with Stickstoff of 0.1 - 0.22 % |