Chemical properties
Property | Value | Comment | |
---|---|---|---|
Chrom | 24 - 26 % Show Supplier Material materials with Chrom of 24 - 26 % | ||
Eisen | Balance | ||
Kohlenstoff | 0.03 % Show Supplier Material materials with Kohlenstoff of 0.03 % | ||
Mangan | 2 % Show Supplier Material materials with Mangan of 2 % | ||
Molybdän | 1.2 - 2 % Show Supplier Material materials with Molybdän of 1.2 - 2 % | ||
Nickel | 5.5 - 6.5 % Show Supplier Material materials with Nickel of 5.5 - 6.5 % | ||
Phosphor | 0.05 % Show Supplier Material materials with Phosphor of 0.05 % | ||
Schwefel | 0.03 % Show Supplier Material materials with Schwefel of 0.03 % | ||
Silizium | 1 % Show Supplier Material materials with Silizium of 1 % | max. | |
Stickstoff | 0.14 - 0.2 % Show Supplier Material materials with Stickstoff of 0.14 - 0.2 % |