Chemical properties
Property | Value | Comment | |
---|---|---|---|
Chrom | 17 - 19 % Show Supplier Material materials with Chrom of 17 - 19 % | ||
Eisen | Balance | ||
Kohlenstoff | 0.08 % Show Supplier Material materials with Kohlenstoff of 0.08 % | ||
Mangan | 2 % Show Supplier Material materials with Mangan of 2 % | ||
Nickel | 9 - 12 % Show Supplier Material materials with Nickel of 9 - 12 % | ||
Phosphor | 0.05 % Show Supplier Material materials with Phosphor of 0.05 % | ||
Schwefel | 0.03 % Show Supplier Material materials with Schwefel of 0.03 % | ||
Silizium | 1 % Show Supplier Material materials with Silizium of 1 % | max. |