Chemical properties
Property | Value | Comment |
---|---|---|
Chrom | 11.5 - 13.5 % Show Supplier Material materials with Chrom of 11.5 - 13.5 % | |
Eisen | 83.1 - 88.4 % Show Supplier Material materials with Eisen of 83.1 - 88.4 % | |
Kohlenstoff | 0.08 - 0.15 % Show Supplier Material materials with Kohlenstoff of 0.08 - 0.15 % | |
Mangan | 1.5 % Show Supplier Material materials with Mangan of 1.5 % | max. |
Nickel | 0.75 % Show Supplier Material materials with Nickel of 0.75 % | |
Phosphor | 0.04 % Show Supplier Material materials with Phosphor of 0.04 % | |
Schwefel | 0 - 0.03 % Show Supplier Material materials with Schwefel of 0 - 0.03 % | |
Silizium | 1 % Show Supplier Material materials with Silizium of 1 % | max. |