Chemical properties
Property | Value | Comment | |
---|---|---|---|
Chrom | 11.5 - 13.5 % Show Supplier Material materials with Chrom of 11.5 - 13.5 % | ||
Eisen | Balance | ||
Kohlenstoff | 0.08 % Show Supplier Material materials with Kohlenstoff of 0.08 % | ||
Mangan | 1 % Show Supplier Material materials with Mangan of 1 % | max. | |
Nickel | 0.6 % Show Supplier Material materials with Nickel of 0.6 % | ||
Phosphor | 0.04 % Show Supplier Material materials with Phosphor of 0.04 % | ||
Schwefel | 0.03 % Show Supplier Material materials with Schwefel of 0.03 % | ||
Silizium | 1 % Show Supplier Material materials with Silizium of 1 % | max. |