Chemical properties
Property | Value | Comment |
---|---|---|
Chrom | 12 - 14 % Show Supplier Material materials with Chrom of 12 - 14 % | |
Eisen | 82.4 - 87.9 % Show Supplier Material materials with Eisen of 82.4 - 87.9 % | |
Kohlenstoff | 0.15 % Show Supplier Material materials with Kohlenstoff of 0.15 % | |
Mangan | 1.5 % Show Supplier Material materials with Mangan of 1.5 % | max. |
Molybdän | 0.6 % Show Supplier Material materials with Molybdän of 0.6 % | |
Phosphor | 0.06 % Show Supplier Material materials with Phosphor of 0.06 % | |
Schwefel | 0.15 - 0.35 % Show Supplier Material materials with Schwefel of 0.15 - 0.35 % | |
Silizium | 1 % Show Supplier Material materials with Silizium of 1 % | max. |