Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 7.8 g/cm³ Show Supplier Material materials with Dichte of 7.8 g/cm³ | typical for steels |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Dehnung A5 | 23.0 °C | 12 - 13 % Show Supplier Material materials with Dehnung A5 of 12 - 13 % | |
Elastizitätsmodul | 23.0 °C | 200 - 210 GPa Show Supplier Material materials with Elastizitätsmodul of 200 - 210 GPa | typical for steels |
Härte, Brinell | 23.0 °C | 230 [-] Show Supplier Material materials with Härte, Brinell of 230 [-] | |
Streckgrenze Rp 0,2 | 23.0 °C | 500 MPa Show Supplier Material materials with Streckgrenze Rp 0,2 of 500 MPa | |
Zugfestigkeit | 23.0 °C | 700 - 950 MPa Show Supplier Material materials with Zugfestigkeit of 700 - 950 MPa |
Chemical properties
Property | Value | Comment |
---|---|---|
Chrom | 12 - 14 % Show Supplier Material materials with Chrom of 12 - 14 % | |
Eisen | 82.3 - 87.9 % Show Supplier Material materials with Eisen of 82.3 - 87.9 % | |
Kohlenstoff | 0.15 - 0.4 % Show Supplier Material materials with Kohlenstoff of 0.15 - 0.4 % | |
Mangan | 1.5 % Show Supplier Material materials with Mangan of 1.5 % | max. |
Molybdän | 0.5 % Show Supplier Material materials with Molybdän of 0.5 % | |
Nickel | 0.75 % Show Supplier Material materials with Nickel of 0.75 % | |
Phosphor | 0.04 % Show Supplier Material materials with Phosphor of 0.04 % | |
Schwefel | 0.03 % Show Supplier Material materials with Schwefel of 0.03 % | |
Silizium | 1 % Show Supplier Material materials with Silizium of 1 % | max. |