Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 7.8 g/cm³ Show Supplier Material materials with Dichte of 7.8 g/cm³ | typical for steels |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Dehnung A5 | 23.0 °C | 10 - 12 % Show Supplier Material materials with Dehnung A5 of 10 - 12 % | |
Elastizitätsmodul | 23.0 °C | 200 - 210 GPa Show Supplier Material materials with Elastizitätsmodul of 200 - 210 GPa | typical for steels |
Härte, Brinell | 23.0 °C | 220 [-] Show Supplier Material materials with Härte, Brinell of 220 [-] | |
Streckgrenze Rp 0,2 | 23.0 °C | 500 MPa Show Supplier Material materials with Streckgrenze Rp 0,2 of 500 MPa | |
Zugfestigkeit | 23.0 °C | 650 - 850 MPa Show Supplier Material materials with Zugfestigkeit of 650 - 850 MPa |
Chemical properties
Property | Value | Comment |
---|---|---|
Chrom | 15.5 - 17.5 % Show Supplier Material materials with Chrom of 15.5 - 17.5 % | |
Kohlenstoff | 0.17 % Show Supplier Material materials with Kohlenstoff of 0.17 % | |
Mangan | 1.5 % Show Supplier Material materials with Mangan of 1.5 % | max. |
Molybdän | 0.2 - 0.6 % Show Supplier Material materials with Molybdän of 0.2 - 0.6 % | |
Schwefel | 0.15 - 0.35 % Show Supplier Material materials with Schwefel of 0.15 - 0.35 % | |
Silizium | 1 % Show Supplier Material materials with Silizium of 1 % | max. |