Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 7.8 g/cm³ Show Supplier Material materials with Dichte of 7.8 g/cm³ | typical for steels |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Dehnung A5 | 23.0 °C | 12 - 14 % Show Supplier Material materials with Dehnung A5 of 12 - 14 % | |
Elastizitätsmodul | 23.0 °C | 200 - 210 GPa Show Supplier Material materials with Elastizitätsmodul of 200 - 210 GPa | typical for steels |
Härte, Brinell | 23.0 °C | 295 [-] Show Supplier Material materials with Härte, Brinell of 295 [-] | |
Streckgrenze Rp 0,2 | 23.0 °C | 600 MPa Show Supplier Material materials with Streckgrenze Rp 0,2 of 600 MPa | |
Zugfestigkeit | 23.0 °C | 800 - 950 MPa Show Supplier Material materials with Zugfestigkeit of 800 - 950 MPa |
Chemical properties
Property | Value | Comment |
---|---|---|
Chrom | 15 - 17 % Show Supplier Material materials with Chrom of 15 - 17 % | |
Eisen | 77.7 - 83.8 % Show Supplier Material materials with Eisen of 77.7 - 83.8 % | |
Kohlenstoff | 0.22 % Show Supplier Material materials with Kohlenstoff of 0.22 % | |
Mangan | 1.5 % Show Supplier Material materials with Mangan of 1.5 % | max. |
Nickel | 1.3 - 2.5 % Show Supplier Material materials with Nickel of 1.3 - 2.5 % | |
Phosphor | 0.04 % Show Supplier Material materials with Phosphor of 0.04 % | |
Schwefel | 0.03 % Show Supplier Material materials with Schwefel of 0.03 % | |
Silizium | 1 % Show Supplier Material materials with Silizium of 1 % | max. |