Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 7.8 g/cm³ Show Supplier Material materials with Dichte of 7.8 g/cm³ | typical for steels |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Dehnung A5 | 23.0 °C | 18 % Show Supplier Material materials with Dehnung A5 of 18 % | |
Elastizitätsmodul | 23.0 °C | 200 - 210 GPa Show Supplier Material materials with Elastizitätsmodul of 200 - 210 GPa | typical for steels |
Härte, Brinell | 23.0 °C | 265 [-] Show Supplier Material materials with Härte, Brinell of 265 [-] | |
Streckgrenze Rp 0,2 | 23.0 °C | 430 MPa Show Supplier Material materials with Streckgrenze Rp 0,2 of 430 MPa | |
Zugfestigkeit | 23.0 °C | 730 - 750 MPa Show Supplier Material materials with Zugfestigkeit of 730 - 750 MPa |
Chemical properties
Property | Value | Comment |
---|---|---|
Chrom | 16 - 19 % Show Supplier Material materials with Chrom of 16 - 19 % | |
Eisen | 76.6 - 83.3 % Show Supplier Material materials with Eisen of 76.6 - 83.3 % | |
Kohlenstoff | 0.75 - 1 % Show Supplier Material materials with Kohlenstoff of 0.75 - 1 % | |
Mangan | 1 % Show Supplier Material materials with Mangan of 1 % | max. |
Molybdän | 1.3 % Show Supplier Material materials with Molybdän of 1.3 % | |
Phosphor | 0.04 % Show Supplier Material materials with Phosphor of 0.04 % | |
Schwefel | 0.02 % Show Supplier Material materials with Schwefel of 0.02 % | |
Silizium | 1 % Show Supplier Material materials with Silizium of 1 % | max. |
Vanadium | 0.07 - 0.12 % Show Supplier Material materials with Vanadium of 0.07 - 0.12 % |