Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 7.8 g/cm³ Show Supplier Material materials with Dichte of 7.8 g/cm³ | typical for steels |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Dehnung A5 | 23.0 °C | 13 % Show Supplier Material materials with Dehnung A5 of 13 % | |
Elastizitätsmodul | 23.0 °C | 200 - 210 GPa Show Supplier Material materials with Elastizitätsmodul of 200 - 210 GPa | typical for steels |
Härte, Brinell | 23.0 °C | 285 [-] Show Supplier Material materials with Härte, Brinell of 285 [-] | |
Streckgrenze Rp 0,2 | 23.0 °C | 445 MPa Show Supplier Material materials with Streckgrenze Rp 0,2 of 445 MPa | |
Zugfestigkeit | 23.0 °C | 740 - 755 MPa Show Supplier Material materials with Zugfestigkeit of 740 - 755 MPa |
Chemical properties
Property | Value | Comment |
---|---|---|
Chrom | 16 - 18 % Show Supplier Material materials with Chrom of 16 - 18 % | |
Eisen | 78 - 83.1 % Show Supplier Material materials with Eisen of 78 - 83.1 % | |
Kohlenstoff | 1 - 1.2 % Show Supplier Material materials with Kohlenstoff of 1 - 1.2 % | |
Mangan | 1 % Show Supplier Material materials with Mangan of 1 % | max. |
Molybdän | 0.8 % Show Supplier Material materials with Molybdän of 0.8 % | |
Phosphor | 0.04 % Show Supplier Material materials with Phosphor of 0.04 % | |
Schwefel | 0.02 % Show Supplier Material materials with Schwefel of 0.02 % | |
Silizium | 1 % Show Supplier Material materials with Silizium of 1 % | max. |