Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 7.8 g/cm³ Show Supplier Material materials with Dichte of 7.8 g/cm³ | typical for steels |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Dehnung A5 | 23.0 °C | 12 % Show Supplier Material materials with Dehnung A5 of 12 % | |
Elastizitätsmodul | 23.0 °C | 200 - 210 GPa Show Supplier Material materials with Elastizitätsmodul of 200 - 210 GPa | typical for steels |
Härte, Brinell | 23.0 °C | 352 [-] Show Supplier Material materials with Härte, Brinell of 352 [-] | |
Streckgrenze Rp 0,2 | 23.0 °C | 1000 MPa Show Supplier Material materials with Streckgrenze Rp 0,2 of 1000 MPa | |
Zugfestigkeit | 23.0 °C | 1070 - 1100 MPa Show Supplier Material materials with Zugfestigkeit of 1070 - 1100 MPa |
Chemical properties
Property | Value | Comment |
---|---|---|
Chrom | 15 - 17 % Show Supplier Material materials with Chrom of 15 - 17 % | |
Kohlenstoff | 0.07 % Show Supplier Material materials with Kohlenstoff of 0.07 % | max. |
Kupfer | 3 - 5 % Show Supplier Material materials with Kupfer of 3 - 5 % | |
Mangan | 1.5 % Show Supplier Material materials with Mangan of 1.5 % | max. |
Molybdän | 0 - 0.6 % Show Supplier Material materials with Molybdän of 0 - 0.6 % | |
Nickel | 3 - 5 % Show Supplier Material materials with Nickel of 3 - 5 % | |
Niobium | 0 - 0.45 % Show Supplier Material materials with Niobium of 0 - 0.45 % | 5x%C |
Silizium | 0.7 % Show Supplier Material materials with Silizium of 0.7 % | max. |