Chemical properties
Property | Value | Comment |
---|---|---|
Aluminium | 0.75 - 1.5 % Show Supplier Material materials with Aluminium of 0.75 - 1.5 % | |
Chrom | 16 - 18 % Show Supplier Material materials with Chrom of 16 - 18 % | |
Eisen | 70.58 - 76.75 % Show Supplier Material materials with Eisen of 70.58 - 76.75 % | Balance |
Kohlenstoff | 0.09 % Show Supplier Material materials with Kohlenstoff of 0.09 % | |
Mangan | 1 % Show Supplier Material materials with Mangan of 1 % | |
Nickel | 6.5 - 7.75 % Show Supplier Material materials with Nickel of 6.5 - 7.75 % | |
Phosphor | 0.04 % Show Supplier Material materials with Phosphor of 0.04 % | |
Schwefel | 0.03 % Show Supplier Material materials with Schwefel of 0.03 % | |
Silizium | 1 % Show Supplier Material materials with Silizium of 1 % |