Chemical properties
Property | Value |
---|---|
Aluminium | 0.75 - 1.5 % Show Supplier Material materials with Aluminium of 0.75 - 1.5 % |
Chrom | 14 - 16 % Show Supplier Material materials with Chrom of 14 - 16 % |
Eisen | Balance |
Kohlenstoff | 0.09 % Show Supplier Material materials with Kohlenstoff of 0.09 % |
Mangan | 1 % Show Supplier Material materials with Mangan of 1 % |
Molybdän | 2 - 3 % Show Supplier Material materials with Molybdän of 2 - 3 % |
Nickel | 6.5 - 7.7 % Show Supplier Material materials with Nickel of 6.5 - 7.7 % |
Phosphor | 0.04 % Show Supplier Material materials with Phosphor of 0.04 % |
Schwefel | 0.03 % Show Supplier Material materials with Schwefel of 0.03 % |
Silizium | 1 % Show Supplier Material materials with Silizium of 1 % |