Chemical properties
Property | Value |
---|---|
Chrom | 19 - 23 % Show Supplier Material materials with Chrom of 19 - 23 % |
Eisen | Balance |
Kohlenstoff | 0.02 % Show Supplier Material materials with Kohlenstoff of 0.02 % |
Kupfer | 1 - 2 % Show Supplier Material materials with Kupfer of 1 - 2 % |
Mangan | 2 % Show Supplier Material materials with Mangan of 2 % |
Molybdän | 4 - 5 % Show Supplier Material materials with Molybdän of 4 - 5 % |
Nickel | 23 - 28 % Show Supplier Material materials with Nickel of 23 - 28 % |
Phosphor | 0.05 % Show Supplier Material materials with Phosphor of 0.05 % |
Schwefel | 0.04 % Show Supplier Material materials with Schwefel of 0.04 % |
Silizium | 1 % Show Supplier Material materials with Silizium of 1 % |
Stickstoff | 0.1 % Show Supplier Material materials with Stickstoff of 0.1 % |