Chemical properties
Property | Value |
---|---|
Chrom | 19.5 - 20.5 % Show Supplier Material materials with Chrom of 19.5 - 20.5 % |
Eisen | Balance |
Kohlenstoff | 0.02 % Show Supplier Material materials with Kohlenstoff of 0.02 % |
Kupfer | 0.5 - 1 % Show Supplier Material materials with Kupfer of 0.5 - 1 % |
Mangan | 1 % Show Supplier Material materials with Mangan of 1 % |
Molybdän | 6 - 6.5 % Show Supplier Material materials with Molybdän of 6 - 6.5 % |
Nickel | 17.5 - 18.5 % Show Supplier Material materials with Nickel of 17.5 - 18.5 % |
Phosphor | 0.03 % Show Supplier Material materials with Phosphor of 0.03 % |
Schwefel | 0.01 % Show Supplier Material materials with Schwefel of 0.01 % |
Silizium | 0.8 % Show Supplier Material materials with Silizium of 0.8 % |
Stickstoff | 0.18 - 0.22 % Show Supplier Material materials with Stickstoff of 0.18 - 0.22 % |