Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 7.8 g/cm³ Show Supplier Material materials with Dichte of 7.8 g/cm³ | typical for steels |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Dehnung A5 | 23.0 °C | 25 % Show Supplier Material materials with Dehnung A5 of 25 % | |
Elastizitätsmodul | 23.0 °C | 200 - 210 GPa Show Supplier Material materials with Elastizitätsmodul of 200 - 210 GPa | typical for steels |
Härte, Brinell | 23.0 °C | 270 [-] Show Supplier Material materials with Härte, Brinell of 270 [-] | |
Streckgrenze Rp 0,2 | 23.0 °C | 450 MPa Show Supplier Material materials with Streckgrenze Rp 0,2 of 450 MPa | |
Zugfestigkeit | 23.0 °C | 650 - 880 MPa Show Supplier Material materials with Zugfestigkeit of 650 - 880 MPa |
Chemical properties
Property | Value | Comment |
---|---|---|
Chrom | 21 - 23 % Show Supplier Material materials with Chrom of 21 - 23 % | |
Kohlenstoff | 0.03 % Show Supplier Material materials with Kohlenstoff of 0.03 % | max. |
Mangan | 2 % Show Supplier Material materials with Mangan of 2 % | max. |
Molybdän | 2.5 - 3.5 % Show Supplier Material materials with Molybdän of 2.5 - 3.5 % | |
Nickel | 4.5 - 6.5 % Show Supplier Material materials with Nickel of 4.5 - 6.5 % | |
Silizium | 1 % Show Supplier Material materials with Silizium of 1 % | max. |
Stickstoff | 0.1 - 0.22 % Show Supplier Material materials with Stickstoff of 0.1 - 0.22 % |