Chemical properties
Property | Value |
---|---|
Aluminium | 0.5 - 1 % Show Supplier Material materials with Aluminium of 0.5 - 1 % |
Chrom | 6 - 8 % Show Supplier Material materials with Chrom of 6 - 8 % |
Eisen | Balance |
Kohlenstoff | 0.12 % Show Supplier Material materials with Kohlenstoff of 0.12 % |
Mangan | 1 % Show Supplier Material materials with Mangan of 1 % |
Phosphor | 0.04 % Show Supplier Material materials with Phosphor of 0.04 % |
Schwefel | 0.02 % Show Supplier Material materials with Schwefel of 0.02 % |
Silizium | 0.5 - 1 % Show Supplier Material materials with Silizium of 0.5 - 1 % |