Chemical properties
Property | Value |
---|---|
Chrom | 23 - 27 % Show Supplier Material materials with Chrom of 23 - 27 % |
Eisen | Balance |
Kohlenstoff | 0.2 % Show Supplier Material materials with Kohlenstoff of 0.2 % |
Mangan | 1.5 % Show Supplier Material materials with Mangan of 1.5 % |
Nickel | 0.75 % Show Supplier Material materials with Nickel of 0.75 % |
Phosphor | 0.04 % Show Supplier Material materials with Phosphor of 0.04 % |
Schwefel | 0.03 % Show Supplier Material materials with Schwefel of 0.03 % |
Silizium | 1 % Show Supplier Material materials with Silizium of 1 % |
Stickstoff | 0.25 % Show Supplier Material materials with Stickstoff of 0.25 % |