Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 7.8 g/cm³ Show Supplier Material materials with Dichte of 7.8 g/cm³ | typical for steels |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Dehnung A5 | 23.0 °C | 30 % Show Supplier Material materials with Dehnung A5 of 30 % | |
Elastizitätsmodul | 23.0 °C | 200 - 210 GPa Show Supplier Material materials with Elastizitätsmodul of 200 - 210 GPa | typical for steels |
Härte, Brinell | 23.0 °C | 223 [-] Show Supplier Material materials with Härte, Brinell of 223 [-] | |
Streckgrenze Rp 0,2 | 23.0 °C | 230 MPa Show Supplier Material materials with Streckgrenze Rp 0,2 of 230 MPa | |
Zugfestigkeit | 23.0 °C | 500 - 750 MPa Show Supplier Material materials with Zugfestigkeit of 500 - 750 MPa |
Chemical properties
Property | Value | Comment |
---|---|---|
Chrom | 19 - 24 % Show Supplier Material materials with Chrom of 19 - 24 % | |
Eisen | 58 - 68.5 % Show Supplier Material materials with Eisen of 58 - 68.5 % | |
Kohlenstoff | 0.2 % Show Supplier Material materials with Kohlenstoff of 0.2 % | |
Mangan | 2 % Show Supplier Material materials with Mangan of 2 % | max. |
Nickel | 11 - 15 % Show Supplier Material materials with Nickel of 11 - 15 % | |
Phosphor | 0.05 % Show Supplier Material materials with Phosphor of 0.05 % | |
Schwefel | 0.03 % Show Supplier Material materials with Schwefel of 0.03 % | |
Silizium | 2.5 % Show Supplier Material materials with Silizium of 2.5 % | max. |
Stickstoff | 0.1 % Show Supplier Material materials with Stickstoff of 0.1 % |