Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 7.8 g/cm³ Show Supplier Material materials with Dichte of 7.8 g/cm³ | typical for steels |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Dehnung A5 | 23.0 °C | 30 % Show Supplier Material materials with Dehnung A5 of 30 % | |
Elastizitätsmodul | 23.0 °C | 200 - 210 GPa Show Supplier Material materials with Elastizitätsmodul of 200 - 210 GPa | typical for steels |
Härte, Brinell | 23.0 °C | 223 [-] Show Supplier Material materials with Härte, Brinell of 223 [-] | |
Streckgrenze Rp 0,2 | 23.0 °C | 230 MPa Show Supplier Material materials with Streckgrenze Rp 0,2 of 230 MPa | |
Zugfestigkeit | 23.0 °C | 550 - 800 MPa Show Supplier Material materials with Zugfestigkeit of 550 - 800 MPa |
Chemical properties
Property | Value | Comment |
---|---|---|
Chrom | 24 - 26 % Show Supplier Material materials with Chrom of 24 - 26 % | |
Kohlenstoff | 0.2 % Show Supplier Material materials with Kohlenstoff of 0.2 % | max. |
Mangan | 2 % Show Supplier Material materials with Mangan of 2 % | max. |
Nickel | 19 - 22 % Show Supplier Material materials with Nickel of 19 - 22 % | |
Schwefel | 1.5 - 2.5 % Show Supplier Material materials with Schwefel of 1.5 - 2.5 % | |
Silizium | 2.5 % Show Supplier Material materials with Silizium of 2.5 % | max. |