Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 7.8 g/cm³ Show Supplier Material materials with Dichte of 7.8 g/cm³ | typical for steels |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Dehnung A5 | 23.0 °C | 35 % Show Supplier Material materials with Dehnung A5 of 35 % | |
Elastizitätsmodul | 23.0 °C | 200 - 210 GPa Show Supplier Material materials with Elastizitätsmodul of 200 - 210 GPa | typical for steels |
Härte, Brinell | 23.0 °C | 192 [-] Show Supplier Material materials with Härte, Brinell of 192 [-] | |
Streckgrenze Rp 0,2 | 23.0 °C | 210 MPa Show Supplier Material materials with Streckgrenze Rp 0,2 of 210 MPa | |
Zugfestigkeit | 23.0 °C | 500 - 750 MPa Show Supplier Material materials with Zugfestigkeit of 500 - 750 MPa |
Chemical properties
Property | Value | Comment |
---|---|---|
Chrom | 24 - 26 % Show Supplier Material materials with Chrom of 24 - 26 % | |
Kohlenstoff | 0.15 % Show Supplier Material materials with Kohlenstoff of 0.15 % | max. |
Mangan | 2 % Show Supplier Material materials with Mangan of 2 % | max. |
Nickel | 19 - 22 % Show Supplier Material materials with Nickel of 19 - 22 % | |
Schwefel | 0 - 0.75 % Show Supplier Material materials with Schwefel of 0 - 0.75 % | |
Silizium | 1.5 % Show Supplier Material materials with Silizium of 1.5 % | max. |