Chemical properties
Property | Value |
---|---|
Cerium | 0.03 - 0.08 % Show Supplier Material materials with Cerium of 0.03 - 0.08 % |
Chrom | 20 - 22 % Show Supplier Material materials with Chrom of 20 - 22 % |
Eisen | 62 - 68.4 % Show Supplier Material materials with Eisen of 62 - 68.4 % |
Kohlenstoff | 0.05 - 0.12 % Show Supplier Material materials with Kohlenstoff of 0.05 - 0.12 % |
Mangan | 1 % Show Supplier Material materials with Mangan of 1 % |
Nickel | 10 - 12 % Show Supplier Material materials with Nickel of 10 - 12 % |
Phosphor | 0 - 0.05 % Show Supplier Material materials with Phosphor of 0 - 0.05 % |
Schwefel | 0 - 0.03 % Show Supplier Material materials with Schwefel of 0 - 0.03 % |
Silizium | 1.4 - 2.5 % Show Supplier Material materials with Silizium of 1.4 - 2.5 % |
Stickstoff | 0.12 - 0.2 % Show Supplier Material materials with Stickstoff of 0.12 - 0.2 % |