Mechanisch
Property | Temperature | Value |
---|---|---|
Dehnung A5 | 23.0 °C | 20 - 24 % Show Supplier Material materials with Dehnung A5 of 20 - 24 % |
Härte, Brinell | 23.0 °C | 190 [-] Show Supplier Material materials with Härte, Brinell of 190 [-] |
Streckgrenze Rp 0,2 | 23.0 °C | 275 MPa Show Supplier Material materials with Streckgrenze Rp 0,2 of 275 MPa |
Zugfestigkeit | 23.0 °C | 345 - 450 MPa Show Supplier Material materials with Zugfestigkeit of 345 - 450 MPa |
Chemical properties
Property | Value |
---|---|
Eisen | 0.3 % Show Supplier Material materials with Eisen of 0.3 % |
Kohlenstoff | 0.08 % Show Supplier Material materials with Kohlenstoff of 0.08 % |
Sauerstoff | 0.25 % Show Supplier Material materials with Sauerstoff of 0.25 % |
Stickstoff | 0.03 % Show Supplier Material materials with Stickstoff of 0.03 % |
Titan | Balance |
Wasserstoff | 0.02 % Show Supplier Material materials with Wasserstoff of 0.02 % |