Allgemein
Property | Temperature | Value |
---|---|---|
Dichte | 23.0 °C | 8.9 g/cm³ Show Supplier Material materials with Dichte of 8.9 g/cm³ |
Chemical properties
Property | Value | Comment |
---|---|---|
Eisen | 0.4 % Show Supplier Material materials with Eisen of 0.4 % | max. |
Kohlenstoff | 0.02 % Show Supplier Material materials with Kohlenstoff of 0.02 % | max. |
Kupfer | 0.25 % Show Supplier Material materials with Kupfer of 0.25 % | |
Magnesium | 0.15 % Show Supplier Material materials with Magnesium of 0.15 % | |
Mangan | 0.35 % Show Supplier Material materials with Mangan of 0.35 % | max. |
Nickel | 99 % Show Supplier Material materials with Nickel of 99 % | min. |
Schwefel | 5E-3 % Show Supplier Material materials with Schwefel of 5E-3 % | max. |
Silizium | 0.25 % Show Supplier Material materials with Silizium of 0.25 % | max. |
Titan | 0.1 % Show Supplier Material materials with Titan of 0.1 % | max. |