Allgemein
Property | Temperature | Value |
---|---|---|
Dichte | 23.0 °C | 9.3 g/cm³ Show Supplier Material materials with Dichte of 9.3 g/cm³ |
Chemical properties
Property | Value | Comment |
---|---|---|
Aluminium | 0.1 - 0.5 % Show Supplier Material materials with Aluminium of 0.1 - 0.5 % | |
Andere | 0.4 % Show Supplier Material materials with Andere of 0.4 % | Nb + Ta |
Chrom | 0.5 - 3 % Show Supplier Material materials with Chrom of 0.5 - 3 % | |
Eisen | 1 - 6 % Show Supplier Material materials with Eisen of 1 - 6 % | |
Kobalt | 3 % Show Supplier Material materials with Kobalt of 3 % | max. |
Kohlenstoff | 0.01 % Show Supplier Material materials with Kohlenstoff of 0.01 % | max. |
Kupfer | 0.5 % Show Supplier Material materials with Kupfer of 0.5 % | |
Mangan | 3 % Show Supplier Material materials with Mangan of 3 % | max. |
Molybdän | 26 - 32 % Show Supplier Material materials with Molybdän of 26 - 32 % | |
Nickel | 65 % Show Supplier Material materials with Nickel of 65 % | min. |
Phosphor | 0.03 % Show Supplier Material materials with Phosphor of 0.03 % | max. |
Schwefel | 0.015 % Show Supplier Material materials with Schwefel of 0.015 % | max. |
Silizium | 0.1 % Show Supplier Material materials with Silizium of 0.1 % | max. |
Titan | 0.2 % Show Supplier Material materials with Titan of 0.2 % | max. |
Vanadium | 0.2 % Show Supplier Material materials with Vanadium of 0.2 % | |
Wolfram | 3 % Show Supplier Material materials with Wolfram of 3 % | max. |