Allgemein
Property | Temperature | Value |
---|---|---|
Dichte | 23.0 °C | 8.7 g/cm³ Show Supplier Material materials with Dichte of 8.7 g/cm³ |
Chemical properties
Property | Value | Comment | |
---|---|---|---|
Chrom | 14 - 18 % Show Supplier Material materials with Chrom of 14 - 18 % | ||
Eisen | 3 % Show Supplier Material materials with Eisen of 3 % | max. | |
Kobalt | 2 % Show Supplier Material materials with Kobalt of 2 % | max. | |
Kohlenstoff | 0.015 % Show Supplier Material materials with Kohlenstoff of 0.015 % | max. | |
Kupfer | 0.5 % Show Supplier Material materials with Kupfer of 0.5 % | ||
Mangan | 1 % Show Supplier Material materials with Mangan of 1 % | max. | |
Molybdän | 14 - 17 % Show Supplier Material materials with Molybdän of 14 - 17 % | ||
Nickel | balance | ||
Phosphor | 0.03 % Show Supplier Material materials with Phosphor of 0.03 % | max. | |
Schwefel | 0.015 % Show Supplier Material materials with Schwefel of 0.015 % | max. | |
Silizium | 0.08 % Show Supplier Material materials with Silizium of 0.08 % | max. | |
Titan | 0.7 % Show Supplier Material materials with Titan of 0.7 % | max. |