Allgemein
Property | Temperature | Value |
---|---|---|
Dichte | 23.0 °C | 8.7 g/cm³ Show Supplier Material materials with Dichte of 8.7 g/cm³ |
Chemical properties
Property | Value | Comment | |
---|---|---|---|
Chrom | 20 - 22.5 % Show Supplier Material materials with Chrom of 20 - 22.5 % | ||
Eisen | 2 - 6 % Show Supplier Material materials with Eisen of 2 - 6 % | ||
Kobalt | 2.5 % Show Supplier Material materials with Kobalt of 2.5 % | max. | |
Kohlenstoff | 0.01 % Show Supplier Material materials with Kohlenstoff of 0.01 % | max. | |
Mangan | 0.5 % Show Supplier Material materials with Mangan of 0.5 % | max. | |
Molybdän | 12.5 - 14.5 % Show Supplier Material materials with Molybdän of 12.5 - 14.5 % | ||
Nickel | balance | ||
Phosphor | 0.03 % Show Supplier Material materials with Phosphor of 0.03 % | max. | |
Schwefel | 0.015 % Show Supplier Material materials with Schwefel of 0.015 % | max. | |
Silizium | 0.08 % Show Supplier Material materials with Silizium of 0.08 % | max. | |
Vanadium | 0.35 % Show Supplier Material materials with Vanadium of 0.35 % | ||
Wolfram | 2.5 - 3.5 % Show Supplier Material materials with Wolfram of 2.5 - 3.5 % |