Allgemein
Property | Temperature | Value |
---|---|---|
Dichte | 23.0 °C | 8.9 g/cm³ Show Supplier Material materials with Dichte of 8.9 g/cm³ |
Chemical properties
Property | Value | Comment | |
---|---|---|---|
Chrom | 14.5 - 16.5 % Show Supplier Material materials with Chrom of 14.5 - 16.5 % | ||
Eisen | 4 - 7 % Show Supplier Material materials with Eisen of 4 - 7 % | ||
Kobalt | 2.5 % Show Supplier Material materials with Kobalt of 2.5 % | max. | |
Kohlenstoff | 0.01 % Show Supplier Material materials with Kohlenstoff of 0.01 % | max. | |
Kupfer | 0.5 % Show Supplier Material materials with Kupfer of 0.5 % | ||
Mangan | 1 % Show Supplier Material materials with Mangan of 1 % | max. | |
Molybdän | 15 - 17 % Show Supplier Material materials with Molybdän of 15 - 17 % | ||
Nickel | balance | ||
Phosphor | 0.02 % Show Supplier Material materials with Phosphor of 0.02 % | max. | |
Schwefel | 0.015 % Show Supplier Material materials with Schwefel of 0.015 % | max. | |
Silizium | 0.08 % Show Supplier Material materials with Silizium of 0.08 % | max. | |
Vanadium | 0.35 % Show Supplier Material materials with Vanadium of 0.35 % | ||
Wolfram | 3 - 4.5 % Show Supplier Material materials with Wolfram of 3 - 4.5 % |