Allgemein
Property | Temperature | Value |
---|---|---|
Dichte | 23.0 °C | 8.6 g/cm³ Show Supplier Material materials with Dichte of 8.6 g/cm³ |
Chemical properties
Property | Value | Comment | |
---|---|---|---|
Aluminium | 0.5 % Show Supplier Material materials with Aluminium of 0.5 % | max. | |
Chrom | 22 - 24 % Show Supplier Material materials with Chrom of 22 - 24 % | ||
Eisen | 3 % Show Supplier Material materials with Eisen of 3 % | max. | |
Kobalt | 2 % Show Supplier Material materials with Kobalt of 2 % | max. | |
Kohlenstoff | 0.01 % Show Supplier Material materials with Kohlenstoff of 0.01 % | max. | |
Kupfer | 1.3 - 1.9 % Show Supplier Material materials with Kupfer of 1.3 - 1.9 % | ||
Mangan | 0.5 % Show Supplier Material materials with Mangan of 0.5 % | max. | |
Molybdän | 15 - 17 % Show Supplier Material materials with Molybdän of 15 - 17 % | ||
Nickel | balance | ||
Phosphor | 0.03 % Show Supplier Material materials with Phosphor of 0.03 % | max. | |
Schwefel | 0.015 % Show Supplier Material materials with Schwefel of 0.015 % | max. | |
Silizium | 0.08 % Show Supplier Material materials with Silizium of 0.08 % | max. |