Allgemein
Property | Temperature | Value |
---|---|---|
Dichte | 23.0 °C | 8.9 g/cm³ Show Supplier Material materials with Dichte of 8.9 g/cm³ |
Chemical properties
Property | Value | Comment |
---|---|---|
Aluminium | 0.5 % Show Supplier Material materials with Aluminium of 0.5 % | max. |
Eisen | 1 - 2.5 % Show Supplier Material materials with Eisen of 1 - 2.5 % | |
Kohlenstoff | 0.15 % Show Supplier Material materials with Kohlenstoff of 0.15 % | max. |
Kupfer | 28 - 34 % Show Supplier Material materials with Kupfer of 28 - 34 % | |
Mangan | 2 % Show Supplier Material materials with Mangan of 2 % | max. |
Nickel | 63 % Show Supplier Material materials with Nickel of 63 % | min. |
Schwefel | 0.02 % Show Supplier Material materials with Schwefel of 0.02 % | max. |
Silizium | 0.5 % Show Supplier Material materials with Silizium of 0.5 % | max. |
Titan | 0.3 % Show Supplier Material materials with Titan of 0.3 % | max. |