Allgemein
Property | Temperature | Value |
---|---|---|
Dichte | 23.0 °C | 8.5 g/cm³ Show Supplier Material materials with Dichte of 8.5 g/cm³ |
Chemical properties
Property | Value | Comment |
---|---|---|
Aluminium | 2.2 - 3.5 % Show Supplier Material materials with Aluminium of 2.2 - 3.5 % | |
Eisen | 0.5 - 2 % Show Supplier Material materials with Eisen of 0.5 - 2 % | |
Kohlenstoff | 0.2 % Show Supplier Material materials with Kohlenstoff of 0.2 % | max. |
Kupfer | 27 - 34 % Show Supplier Material materials with Kupfer of 27 - 34 % | |
Mangan | 1.5 % Show Supplier Material materials with Mangan of 1.5 % | max. |
Nickel | 63 % Show Supplier Material materials with Nickel of 63 % | min. |
Schwefel | 0.015 % Show Supplier Material materials with Schwefel of 0.015 % | max. |
Silizium | 0.5 % Show Supplier Material materials with Silizium of 0.5 % | max. |
Titan | 0.3 - 1 % Show Supplier Material materials with Titan of 0.3 - 1 % |