Allgemein
Property | Temperature | Value |
---|---|---|
Dichte | 23.0 °C | 8.5 g/cm³ Show Supplier Material materials with Dichte of 8.5 g/cm³ |
Chemical properties
Property | Value | Comment |
---|---|---|
Aluminium | 0.3 % Show Supplier Material materials with Aluminium of 0.3 % | max. |
Chrom | 14 - 17 % Show Supplier Material materials with Chrom of 14 - 17 % | |
Eisen | 6 - 10 % Show Supplier Material materials with Eisen of 6 - 10 % | |
Kobalt | 1 % Show Supplier Material materials with Kobalt of 1 % | max. |
Kohlenstoff | 0.025 - 0.1 % Show Supplier Material materials with Kohlenstoff of 0.025 - 0.1 % | |
Kupfer | 0.5 % Show Supplier Material materials with Kupfer of 0.5 % | |
Mangan | 1 % Show Supplier Material materials with Mangan of 1 % | max. |
Nickel | 72 % Show Supplier Material materials with Nickel of 72 % | min. |
Phosphor | 0.02 % Show Supplier Material materials with Phosphor of 0.02 % | max. |
Schwefel | 0.015 % Show Supplier Material materials with Schwefel of 0.015 % | max. |
Silizium | 0.5 % Show Supplier Material materials with Silizium of 0.5 % | max. |
Titan | 0.3 % Show Supplier Material materials with Titan of 0.3 % | max. |