Allgemein
Property | Temperature | Value |
---|---|---|
Dichte | 23.0 °C | 8.2 g/cm³ Show Supplier Material materials with Dichte of 8.2 g/cm³ |
Chemical properties
Property | Value | Comment |
---|---|---|
Aluminium | 1 - 1.7 % Show Supplier Material materials with Aluminium of 1 - 1.7 % | |
Bor | 6E-3 % Show Supplier Material materials with Bor of 6E-3 % | |
Chrom | 21 - 25 % Show Supplier Material materials with Chrom of 21 - 25 % | |
Eisen | 18 % Show Supplier Material materials with Eisen of 18 % | max. |
Kohlenstoff | 0.1 % Show Supplier Material materials with Kohlenstoff of 0.1 % | max. |
Kupfer | 0.5 % Show Supplier Material materials with Kupfer of 0.5 % | |
Mangan | 1 % Show Supplier Material materials with Mangan of 1 % | max. |
Nickel | 58 - 63 % Show Supplier Material materials with Nickel of 58 - 63 % | |
Phosphor | 0.02 % Show Supplier Material materials with Phosphor of 0.02 % | max. |
Schwefel | 0.015 % Show Supplier Material materials with Schwefel of 0.015 % | max. |
Silizium | 0.5 % Show Supplier Material materials with Silizium of 0.5 % | max. |
Titan | 0.5 % Show Supplier Material materials with Titan of 0.5 % | max. |