Allgemein
Property | Temperature | Value |
---|---|---|
Dichte | 23.0 °C | 8.3 g/cm³ Show Supplier Material materials with Dichte of 8.3 g/cm³ |
Chemical properties
Property | Value | Comment | |
---|---|---|---|
Aluminium | 0.3 - 0.7 % Show Supplier Material materials with Aluminium of 0.3 - 0.7 % | ||
Andere | 4.7 - 5.5 % Show Supplier Material materials with Andere of 4.7 - 5.5 % | Nb + Ta | |
Bor | 6E-3 % Show Supplier Material materials with Bor of 6E-3 % | ||
Chrom | 17 - 21 % Show Supplier Material materials with Chrom of 17 - 21 % | ||
Eisen | balance | ||
Kobalt | 1 % Show Supplier Material materials with Kobalt of 1 % | max. | |
Kohlenstoff | 0.02 - 0.08 % Show Supplier Material materials with Kohlenstoff of 0.02 - 0.08 % | ||
Kupfer | 0.3 % Show Supplier Material materials with Kupfer of 0.3 % | ||
Mangan | 0.35 % Show Supplier Material materials with Mangan of 0.35 % | max. | |
Molybdän | 2.8 - 3.3 % Show Supplier Material materials with Molybdän of 2.8 - 3.3 % | ||
Nickel | 50 - 55 % Show Supplier Material materials with Nickel of 50 - 55 % | ||
Phosphor | 0.02 % Show Supplier Material materials with Phosphor of 0.02 % | max. | |
Schwefel | 0.015 % Show Supplier Material materials with Schwefel of 0.015 % | max. | |
Silizium | 0.35 % Show Supplier Material materials with Silizium of 0.35 % | max. | |
Titan | 0.6 - 1.2 % Show Supplier Material materials with Titan of 0.6 - 1.2 % |